SIST EN 1971-2:2012
(Main)Copper and copper alloys - Eddy current test for measuring defects on seamless round copper and copper alloy tubes - Part 2: Test with an internal test coil on the inner surface
Copper and copper alloys - Eddy current test for measuring defects on seamless round copper and copper alloy tubes - Part 2: Test with an internal test coil on the inner surface
This part of this European Standard specifies a procedure for the eddy current test with an internal test coil for measuring defects on the inner surface of seamless round copper and copper alloy tubes. The eddy current test method(s) required, together with the size range and acceptance level, are defined in the relevant product standard. The choice of the method for eddy current test:
- with an encircling test coil on the outer surface according EN 1971-1; or
- with an internal test coil on the inner surface according EN 1971-2;
is at the discretion of the manufacturer if there are no other agreements between the purchaser and the supplier. Especially for finned tubes according to EN 12452 with high fins it is recommended to use eddy current test with internal sensor as described in this standard.
Kupfer und Kupferlegierungen - Wirbelstromprüfung an Rohren zur Messung von Fehlern an nahtlos gezogenen runden Rohren aus Kupfer und Kupferlegierungen - Teil 2: Prüfung mit Innensonde auf der Innenseite
Diese Europäische Norm legt ein Verfahren für die Wirbelstromprüfung von nahtlosen runden Rohren aus Kupfer und Kupferlegierungen mit Innensonde auf der Innenoberfläche fest. Diese Europäische Norm gilt insbesondere für Rippenrohre mit hohen Rippen nach EN 12452. ANMERKUNG Das(Die) geforderte(n) Wirbelstromprüfverfahren sowie der Maßbereich und die Sortiergrenze sind in der entsprechenden Produktnorm festgelegt. Die Wahl des Verfahrens für die Wirbelstromprüfung mit
- umfassender Spule auf der Außenseite nach EN 1971-1; oder
- Innensonde auf der Innenseite nach EN 1971-2; obliegt dem Hersteller, wenn keine anderen Vereinbarungen zwischen Hersteller und Lieferer getroffen wurden. Besonders für Rippenrohre mit hohen Rippen nach EN 12452, wird die Anwendung der Wirbelstromprüfung mit Innensonde, wie in dieser Norm beschrieben, empfohlen.
Cuivre et alliages de cuivre - Méthode de contrôle par courants de Foucault pour le mesurage des défauts des tubes ronds sans soudure en cuivre et alliages de cuivre - Partie 2: Essai avec une bobine interne sur la paroi interne
La présente Norme européenne spécifie un mode opératoire relatif au contrôle par courants de Foucault pour
le mesurage des défauts présents sur la paroi interne des tubes ronds sans soudure en cuivre et alliages de
cuivre, au moyen d’un capteur interne.
La présente Norme européenne s'applique en particulier aux tubes à ailettes avec ailettes hautes selon
l'EN 12452.
NOTE La ou les méthode(s) de contrôle par courants de Foucault requise(s), ainsi que les gammes de dimensions
concernées et le niveau d'acceptation, sont spécifiés dans la norme de produit correspondante.
Le choix de la méthode de contrôle par courants de Foucault :
- avec une bobine encerclante sur la paroi externe selon l’EN 1971-1
ou
- avec un capteur interne sur la paroi interne selon l’EN 1971-2
est laissé à la discrétion du fabricant, sauf accord contraire entre le client et le fournisseur.
Il est recommandé, en particulier pour les tubes à ailettes selon l’EN 12452 avec ailettes hautes, d’utiliser le contrôle par
courants de Foucault avec capteur interne selon la description de la présente norme.
Baker in bakrove zlitine - Metoda preskušanja z vrtinčnimi tokovi za merjenje napak na nevarjenih okroglih ceveh iz bakra in bakrovih zlitin - 2. del: Preskus z notranjo preskusno tuljavo ob notranji površini
Ta del tega evropskega standarda določa postopek za metodo preskušanja z vrtinčnimi tokovi z notranjo preskusno tuljavo za merjenje napak ob notranji površini nevarjenih okroglih cevi iz bakra in bakrovih zlitin. Zahtevane metode preskušanja z vrtinčnimi tokovi ter razpon velikosti in meja sprejemljivosti so določeni v ustreznem standardu za izdelek. Metodo za preskušanje z vrtinčnimi tokovi:
– s preskusno tuljavo, ki obdaja zunanjo površino, v skladu s standardom EN 1971-1; ali
– z notranjo preskusno tuljavo ob notranji površini v skladu s standardom EN 1971-2;
izbere proizvajalec, če ne obstaja drugačen dogovor med kupcem in dobaviteljem.
Preskušanje z vrtinčnimi tokovi z notranjim senzorjem v skladu s tem standardom je priporočeno zlasti za narebričene cevi iz standarda EN 12452 z visokimi rebri..
General Information
Relations
Standards Content (Sample)
2003-01.Slovenski inštitut za standardizacijo. Razmnoževanje celote ali delov tega standarda ni dovoljeno.Kupfer und Kupferlegierungen - Wirbelstromprüfung an Rohren zur Messung von Fehlern an nahtlos gezogenen runden Rohren aus Kupfer und Kupferlegierungen - Teil 2: Prüfung mit Innensonde auf der InnenseiteCuivre et alliages de cuivre - Méthode de contrôle par courants de Foucault pour le mesurage des défauts des tubes ronds sans soudure en cuivre et alliages de cuivre - Partie 2: Essai avec une bobine interne sur la paroi interneCopper and copper alloys - Eddy current test for measuring defects on seamless round copper and copper alloy tubes - Part 2: Test with an internal test coil on the inner surface77.150.30Bakreni izdelkiCopper products23.040.15Cevi iz neželeznih kovinNon-ferrous metal pipesICS:Ta slovenski standard je istoveten z:EN 1971-2:2011SIST EN 1971-2:2012en,fr,de01-februar-2012SIST EN 1971-2:2012SLOVENSKI
STANDARD
SIST EN 1971-2:2012
EUROPEAN STANDARD NORME EUROPÉENNE EUROPÄISCHE NORM
EN 1971-2
December 2011 ICS 23.040.15; 77.150.30 English Version
Copper and copper alloys - Eddy current test for measuring defects on seamless round copper and copper alloy tubes - Part 2: Test with an internal probe on the inner surface
Cuivre et alliages de cuivre - Méthode de contrôle par courants de Foucault pour le mesurage des défauts des tubes ronds sans soudure en cuivre et alliages de cuivre - Partie 2:
Essai avec un capteur interne sur la paroi interne Kupfer und Kupferlegierungen - Wirbelstromprüfung an Rohren zur Messung von Fehlern an nahtlos gezogenen runden Rohren aus Kupfer und Kupferlegierungen - Teil 2: Prüfung mit Innensonde auf der Innenseite This European Standard was approved by CEN on 5 November 2011.
CEN members are bound to comply with the CEN/CENELEC Internal Regulations which stipulate the conditions for giving this European Standard the status of a national standard without any alteration. Up-to-date lists and bibliographical references concerning such national standards may be obtained on application to the CEN-CENELEC Management Centre or to any CEN member.
This European Standard exists in three official versions (English, French, German). A version in any other language made by translation under the responsibility of a CEN member into its own language and notified to the CEN-CENELEC Management Centre has the same status as the official versions.
CEN members are the national standards bodies of Austria, Belgium, Bulgaria, Croatia, Cyprus, Czech Republic, Denmark, Estonia, Finland, France, Germany, Greece, Hungary, Iceland, Ireland, Italy, Latvia, Lithuania, Luxembourg, Malta, Netherlands, Norway, Poland, Portugal, Romania, Slovakia, Slovenia, Spain, Sweden, Switzerland and United Kingdom.
EUROPEAN COMMITTEE FOR STANDARDIZATION
COMITÉ EUROPÉEN DE NORMALISATION EUROPÄISCHES KOMITEE FÜR NORMUNG
Management Centre:
Avenue Marnix 17,
B-1000 Brussels © 2011 CEN All rights of exploitation in any form and by any means reserved worldwide for CEN national Members. Ref. No. EN 1971-2:2011: ESIST EN 1971-2:2012
EN 1971-2:2011 (E) 2 Contents Page Foreword .3Introduction .41 Scope .52 Normative references .53 Terms and definitions .54 General requirements .54.1 Personnel qualification .54.2 Condition of tube to be tested .54.3 Equipment .65 Reference standard tube .66 Acceptance criteria .76.1 Detection of local discontinuities by internal probes systems .76.2 Detection of non-local discontinuities by internal probes systems with lower detection levels .76.3 Other test methods .87 Instrument adjustment .8Bibliography .9 Figures Figure 1 — Simplified representation of eddy current testing using internal probe .6
SIST EN 1971-2:2012
EN 1971-2:2011 (E) 3 Foreword This document (EN 1971-2:2011) has been prepared by Technical Committee CEN/TC 133 “Copper and copper alloys”, the secretariat of which is held by DIN. This European Standard shall be given the status of a national standard, either by publication of an identical text or by endorsement, at the latest by June 2012, and conflicting national standards shall be withdrawn at the latest by June 2012. Attention is drawn to the possibility that some of the elements of this document may be the subject of patent rights. CEN [and/or CENELEC] shall not be held responsible for identifying any or all such patent rights. According to the CEN/CENELEC Internal Regulations, the national standards organizations of the following countries are bound to implement this European Standard: Austria, Belgium, Bulgaria, Croatia, Cyprus, Czech Republic, Denmark, Estonia, Finland, France, Germany, Greece, Hungary, Iceland, Ireland, Italy, Latvia, Lithuania, Luxembourg, Malta, Netherlands, Norway, Poland, Portugal, Romania, Slovakia, Slovenia, Spain, Sweden, Switzerland and the United Kingdom. Within its programme of work, Technical Committee CEN/TC 133 requested CEN/TC 133/WG 3 "Copper tubes (installation and industrial)" to prepare the following document: EN 1971-2, Copper and copper alloys — Eddy current test for measuring defects on seamless round copper and copper alloy tubes — Part 2: Test with an internal probe on the inner surface This is one of two parts of the standard for the eddy current test for measuring defects on seamless round copper and copper alloy tubes. The other part is: EN 1971-1, Copper and copper alloys — Eddy current test for measuring defects on seamless round copper and copper alloy tubes — Part 1:Test with an encircling test coil on the outer surface
SIST EN 1971-2:2012
EN 1971-2:2011 (E) 4 Introduction The eddy current test with internal probe described in this standard has the objective of detecting potential leaks and serious defects in seamless round copper and copper alloy tubes. The eddy current test is able to detect material inhomogeneities and their positions throughout the length of tubes. The eddy current signals of material inhomogeneities are compared with reference signals of artificially produced test defects. It is possible to identify these inhomogeneities on the inner and outer surfaces as well as wi
...
Questions, Comments and Discussion