ASTM C836/C836M-12
(Specification)Standard Specification for High Solids Content, Cold Liquid-Applied Elastomeric Waterproofing Membrane for Use with Separate Wearing Course
Standard Specification for High Solids Content, Cold Liquid-Applied Elastomeric Waterproofing Membrane for Use with Separate Wearing Course
ABSTRACT
This specification describes the required properties and test methods for cold liquid-applied elastomeric-type membranes for waterproofing building decks and walls subject to hydrostatic pressure in building areas to be occupied by personnel, vehicles, or equipment. This specification applies only to a membrane system that will be covered with a separate wearing course, traffic course, or backfill. After application by spreading or spraying, the membrane materials shall cure to form an elastomeric film capable of maintaining a seal against liquid water. Materials shall undergo appropriate tests and conform accordingly to the following requirements: hardness; weight loss; nonvolatile matter content; low temperature crack bridging; film thickness; adhesion-in-peel after water immersion; extensibility after heat aging; and storage stability.
SCOPE
1.1 This specification describes the required properties and test methods for a cold liquid-applied elastomeric-type membrane, one- or two-component, for waterproofing building decks and walls subject to hydrostatic pressure in building areas to be occupied by personnel, vehicles, or equipment. This specification applies only to a membrane system that will be covered with a separate wearing course, traffic course, or backfill.
Note 1—See Guide C898 and Guide C1471 for proper application of membrane.
1.2 There are no ISO standards similar or equivalent to this ASTM standard.
1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
General Information
Relations
Buy Standard
Standards Content (Sample)
NOTICE: This standard has either been superseded and replaced by a new version or withdrawn.
Contact ASTM International (www.astm.org) for the latest information
Designation:C836/C836M −12
StandardSpecification for
High Solids Content, Cold Liquid-Applied Elastomeric
Waterproofing Membrane for Use with Separate Wearing
1
Course
This standard is issued under the fixed designation C836/C836M; the number immediately following the designation indicates the year
of original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval.
A superscript epsilon (´) indicates an editorial change since the last revision or reapproval.
1. Scope C898 Guide for Use of High Solids Content, Cold Liquid-
Applied ElastomericWaterproofing Membrane with Sepa-
1.1 This specification describes the required properties and
rate Wearing Course
test methods for a cold liquid-applied elastomeric-type
C1250 Test Method for Nonvolatile Content of Cold Liquid-
membrane, one- or two-component, for waterproofing building
Applied Elastomeric Waterproofing Membranes
decks and walls subject to hydrostatic pressure in building
C1305 Test Method for Crack Bridging Ability of Liquid-
areastobeoccupiedbypersonnel,vehicles,orequipment.This
Applied Waterproofing Membrane
specification applies only to a membrane system that will be
C1375 Guide for Substrates Used in Testing Building Seals
covered with a separate wearing course, traffic course, or
and Sealants
backfill.
C1471 Guide for the Use of High Solids Content Cold
NOTE 1—See Guide C898 and Guide C1471 for proper application of
Liquid-Applied Elastomeric Waterproofing Membrane on
membrane.
Vertical Surfaces
1.2 There are no ISO standards similar or equivalent to this
C1522 Test Method for Extensibility After Heat Aging of
ASTM standard.
Cold Liquid-Applied Elastomeric Waterproofing Mem-
branes
1.3 The values stated in either SI units or inch-pound units
D2240 Test Method for Rubber Property—Durometer Hard-
are to be regarded separately as standard. The values stated in
ness
each system may not be exact equivalents; therefore, each
system shall be used independently of the other. Combining
3. Terminology
values from the two systems may result in non-conformance
with the standard.
3.1 Definitions—Refer to Terminology C717 for definitions
1.4 This standard does not purport to address all of the
of the terms used in this specification.
safety concerns, if any, associated with its use. It is the
responsibility of the user of this standard to establish appro-
4. Classification
priate safety and health practices and determine the applica-
4.1 Types:
bility of regulatory limitations prior to use.
4.1.1 Type I—A one-component, cold liquid-applied water-
2. Referenced Documents proofing material suitable for immediate application after
2 mixing. Type I products may be used with an accelerator that
2.1 ASTM Standards:
is beneficial but not essential for curing of the membrane.
C717 Terminology of Building Seals and Sealants
4.1.2 Type II—Atwo-component, cold liquid-applied water-
C794 TestMethodforAdhesion-in-PeelofElastomericJoint
proofing material. Combining two components is essential for
Sealants
curing of the membrane.
1
This specification is under the jurisdiction of ASTM Committee D08 on 5. Physical Requirements
Roofing and Waterproofing and is the direct responsibility of Subcommittee D08.22
on Waterproofing and Dampproofing Systems. 5.1 Material—Membrane materials shall cure, after appli-
Current edition approved May 1, 2012. Published May 2012. Originally
cation by spreading or spraying, to form an elastomeric film
approved in 1976. Last previous edition approved in 2011 as C836/C836M – 11a.
capable of maintaining a seal against liquid water.
DOI: 10.1520/C0836_C0836M-12.
2
For referenced ASTM standards, visit the ASTM website, www.astm.org, or
5.2 The physical, mechanical, and performance properties
contact ASTM Customer Service at service@astm.org. For Annual Book of ASTM
of the membrane shall conform to the requirements described
Standards volume information, refer to the standard’s Document Summary page on
the ASTM website. in Table 1.
Copyright © ASTM International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA 19428-2959. United States
1
---------------------- Page: 1 ----------------------
C836/C836M−12
TABLE 1 High Solids Content, Cold Liquid-Applied Elastomeric Waterproofing Membrane Physical Requirements
Property Requirement Test Method
Hardness, Type 00, min 50 D2240 as modified in section 6.5 of
this specification
Weight loss, max, % 20 C1250
Nonvolatile, min, % 80
Low temperature crack bridging no cracking C1305
A
Film thickness (vertical surface), 1.5 ± 0.1 [60 ± 5] See section 6.8 of this specification
min, mm [mils]
Adhesion-in-Peel after water 4.4 [1] C794 as modified in section 6.9 of
immersion, N [lbf] this specification
1
Extensibility after heat aging, min, 6.4 [ ⁄4 ], no cracking C1522
mm [in.]
Stability, min, months 6 See
...
This document is not an ASTM standard and is intended only to provide the user of an ASTM standard an indication of what changes have been made to the previous version. Because
it may not be technically possible to adequately depict all changes accurately, ASTM recommends that users consult prior editions as appropriate. In all cases only the current version
of the standard as published by ASTM is to be considered the official document.
Designation:C836/C836M–11a Designation: C836/C836M – 12
Standard Specification for
High Solids Content, Cold Liquid-Applied Elastomeric
Waterproofing Membrane for Use with Separate Wearing
1
Course
This standard is issued under the fixed designation C836/C836M; the number immediately following the designation indicates the year
of original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval.
A superscript epsilon (´) indicates an editorial change since the last revision or reapproval.
This standard has been approved for use by agencies of the Department of Defense.
1. Scope
1.1 This specification describes the required properties and test methods for a cold liquid-applied elastomeric-type membrane,
one- or two-component, for waterproofing building decks and walls subject to hydrostatic pressure in building areas to be occupied
by personnel, vehicles, or equipment. This specification applies only to a membrane system that will be covered with a separate
wearing course, traffic course, or backfill.
NOTE 1—See Guide C898 and Guide C1471 for proper application of membrane.
1.2 There are no ISO standards similar or equivalent to this ASTM standard.
1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each
system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the
two systems may result in non-conformance with the standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility
of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory
limitations prior to use.
2. Referenced Documents
2
2.1 ASTM Standards:
C717 Terminology of Building Seals and Sealants
C794 Test Method for Adhesion-in-Peel of Elastomeric Joint Sealants
C898 Guide for Use of High Solids Content, Cold Liquid-Applied Elastomeric Waterproofing Membrane with Separate
Wearing Course
C1250 Test Method for Nonvolatile Content of Cold Liquid-Applied Elastomeric Waterproofing Membranes
C1305 Test Method for Crack Bridging Ability of Liquid-Applied Waterproofing Membrane
C1375 Guide for Substrates Used in Testing Building Seals and Sealants
C1471 Guide for the Use of High Solids Content Cold Liquid-Applied Elastomeric Waterproofing Membrane on Vertical
Surfaces
C1522 Test Method for Extensibility After Heat Aging of Cold Liquid-Applied Elastomeric Waterproofing Membranes
D2240 Test Method for Rubber PropertyDurometer Hardness
3. Terminology
3.1 Definitions—Refer to Terminology C717 for definitions of the terms used in this specification.
4. Classification
4.1 Types:
4.1.1 Type I—A one-component, cold liquid-applied waterproofing material suitable for immediate application after mixing.
Type I products may be used with an accelerator that is beneficial but not essential for curing of the membrane.
1
This specification is under the jurisdiction of ASTM Committee D08 on Roofing and Waterproofing and is the direct responsibility of Subcommittee D08.22 on
Waterproofing and Dampproofing Systems.
Current edition approved JulyMay 1, 2011.2012. Published July 2011.May 2012. Originally approved in 1976. Last previous edition approved in 2011 as
C836/C836M – 11a. DOI: 10.1520/C0836_C0836M-11A2.
2
For referencedASTM standards, visit theASTM website, www.astm.org, or contactASTM Customer Service at service@astm.org. For Annual Book of ASTM Standards
volume information, refer to the standard’s Document Summary page on the ASTM website.
Copyright © ASTM International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA 19428-2959, United States.
1
---------------------- Page: 1 ----------------------
C836/C836M – 12
4.1.2 Type II—Atwo-component,coldliquid-appliedwaterproofingmaterial.Combiningtwocomponentsisessentialforcuring
of the membrane.
5. Physical Requirements
5.1 Material—Membrane materials shall cure, after application by spreading or spraying, to form an elastomeric film capable
of maintaining a seal against liquid water.
5.2 The physical, mechanical, and performance properties of the membrane shall conform to the requirements described in
Table 1.
6. Test Methods
6.1 Standard Conditions—Standard conditions for all tests shall be 23 6 2°C [73.4 6 3.6°F] and 50 6 5 % relative humidity.
6.2 Conditioning/Mixing:
6.2.1 Store all membrane materials to be tested in an unopened container at sta
...
Questions, Comments and Discussion
Ask us and Technical Secretary will try to provide an answer. You can facilitate discussion about the standard in here.