(Main)Hard coal -- Determination of caking index
Hard coal -- Determination of caking index
This International Standard specifies a method of determination of caking index of hard coal. It is applicable to the evaluation of caking power of bituminous coal with random reflectance of vitrinite, Rr, greater than 0,6 % and less than or equal to 1,8 % (> 0,6 % u 1,8 %).
Houille -- Détermination de l'indice d'agglutination
Črni premog – Določanje količnika spekavosti
General Information
Buy Standard
Standards Content (Sample)
МЕЖДУНАРОДНЫЙ ISO
СТАНДАРТ 15585
Первое издание
2006-01-15
Уголь каменный. Определение индекса
спекаемости
Hard coal — Determination of caking index
Ответственность за подготовку русской версии несёт GOST R
(Российская Федерация) в соответствии со статьёй 18.1 Устава ISO
Ссылочный номер
ISO 15585:2006(R)
©
ISO 2006
---------------------- Page: 1 ----------------------
ISO 15585:2006(R)
Отказ от ответственности при работе в PDF
Настоящий файл PDF может содержать интегрированные шрифты. В соответствии с условиями лицензирования, принятыми
фирмой Adobe, этот файл можно распечатать или вывести на экран, но его нельзя изменить, пока не будет получена
лицензия на загрузку интегрированных шрифтов в компьютер, на котором ведется редактирование. В случае загрузки
настоящего файла заинтересованные стороны принимают на себя ответственность за соблюдение лицензионных условий
фирмы Adobe. Центральный секретариат ISO не несет никакой ответственности в этом отношении.
Adobe − торговый знак фирмы Adobe Systems Incorporated.
Подробности, относящиеся к программным продуктам, использованным для создания настоящего файла PDF, можно найти в
рубрике General Info файла; параметры создания PDF были оптимизированы для печати. Были приняты во внимание все
меры предосторожности с тем, чтобы обеспечить пригодность настоящего файла для использования комитетами-членами
ISO. В редких случаях возникновения проблемы, связанной со сказанным выше, просьба проинформировать Центральный
секретариат по адресу, приведенному ниже.
ДОКУМЕНТ ЗАЩИЩЕН АВТОРСКИМ ПРАВОМ
© ISO 2006
Все права сохраняются. Если не указано иное, никакую часть настоящей публикации нельзя копировать или использовать в
какой-либо форме или каким-либо электронным или механическим способом, включая фотокопии и микрофильмы, без
предварительного письменного согласия ISO по адресу, указанному ниже, или членов ISO в стране регистрации пребывания.
ISO copyright office
Case postale 56 • CH-1211 Geneva 20
Tel. + 41 22 749 01 11
Fax + 41 22 749 09 47
E-mail copyright@iso.org
Web www.iso.org
Опубликовано в Швейцарии
ii © ISO 2006 – Все права сохраняются
---------------------- Page: 2 ----------------------
ISO 15585:2006(R)
Содержание Страница
Предисловие .iv
1 Область применения .1
2 Нормативные ссылки .1
3 Термины и определения .1
4 Принцип.1
5 Реактив .1
6 Оборудование .2
7 Проба угля.7
8 Процедура.7
9 Расчет результатов.7
10 Дополнительное испытание .8
11 Сходимость.8
12 Протокол испытания.8
Приложение А (информативное) Извлечение и приготовление стандартного антрацита для
определения индекса спекаемости .9
Приложение В (информативное) Проверка качества стандартного антрацита,
используемого для определения индекса спекаемости .10
© ISO 2006 – Все права сохраняются iii
---------------------- Page: 3 ----------------------
ISO 15585:2006(R)
Предисловие
Международная организация по стандартизации (ISO) является всемирной федерацией национальных
организаций по стандартизации (комитетов-членов ISO). Разработка международных стандартов
обычно осуществляется техническими комитетами ISO. Каждый комитет-член, заинтересованный в
деятельности, для которой был создан технический комитет, имеет право быть представленным в этом
комитете. Международные государственные и негосударственные организации, имеющие связи с ISO,
также принимают участие в работах. Что касается стандартизации в области электротехники, то ISO
работает в тесном сотрудничестве с Международной электротехнической комиссией (IEC).
Проекты международных стандартов разрабатываются в соответствии с правилами, установленными в
Директивах ISO/IEC, Часть 2.
Основная задача технических комитетов заключается в подготовке международных стандартов.
Проекты международных стандартов, принятые техническими комитетами, рассылаются комитетам-
членам на голосование. Их опубликование в качестве международных стандартов требует одобрения
не менее 75 % комитетов-членов, принимающих участие в голосовании.
Следует иметь в виду, что некоторые элементы настоящего документа могут быть объектом
патентного права. ISO не может нести ответственность за идентификацию какого-либо одного или всех
патентных прав.
ISO 15585 подготовлен Техническим комитетом ISO/TC 27, Твердое минеральное топливо,
Подкомитетом SC 5, Методы анализа.
iv © ISO 2006 – Все права сохраняются
---------------------- Page: 4 ----------------------
МЕЖДУНАРОДНЫЙ СТАНДАРТ ISO 15585:2006(R)
Уголь каменный. Определение индекса спекаемости
1 Область применения
В настоящем международном стандарте устанавливается метод определения индекса спекаемости
каменного угля. Данный международный стандарт распространяется на оценку битуминозного угля со
стохастической отражательной способностью витринита, R , превышающей 0,6 % и меньшей или
r
равной 1,8 % (> 0,6 % ≤ 1,8 %).
2 Нормативные ссылки
Следующие ссылочные документы являются обязательными при применении данного документа. Для
жестких ссылок применяется только цитированное издание документа. Для плавающих ссылок
необходимо использовать самое последнее издание нормативного ссылочного документа (включая
любые изменения).
ISO 562, Уголь каменный и кокс. Определение содержания летучих веществ
ISO 589, Уголь каменный. Определение полной влажности
ISO 1171, Топливо твердое минеральное. Определение содержания золы
3 Термины и определения
3.1
индекс спекаемости
caking index
мера величины прочности связей между частицами угля или частицами угля и инертными частицами
после нагревания угля при температуре 850 °C.
4 Принцип
Часть приготовленной пробы угля с ограниченной градацией размеров частиц и стандартный антрацит
перемешиваются в установленных условиях, а затем их смесь быстро коксуется. Кокс, полученный
таким способом в тигле, испытывается на прочность в барабане, отвечающим установленным
техническим требованиям. Спекаемость испытательной пробы определяется абразивной прочностью,
т. е. сопротивлением дроблению кокса, полученного в тигле.
5 Реактив
5.1 Стандартный антрацит, содержащий влагу в количестве менее 2,5 массовых % основы,
высушенной на воздухе, золу в количестве менее 4 массовых % сухой основы и летучее вещество в
количестве менее 8 массовых % сухой основы без золы. Предельные размеры частиц составляют от
0,1 мм до 0,2 мм, the содержание частиц размером менее of 0,1 мм должно не превышать
6 массовых %, а содержание частиц размером более 0,2 мм не должно превышать более
4 массовых %.
© ISO 2006 – Все права сохраняются 1
---------------------- Page: 5 ----------------------
ISO 15585:2006(R)
ПРИМЕЧАНИЕ В Приложениях A и B представлена информация по извлечению, приготовлению и испытаниям
стандартного антрацита.
6 Оборудование
6.1 Весы, выполняющие взвешивание с точностью до ближайших 0,01 г.
6.2 Тигель, фарфоровый, имеющий следующие размеры (см. Рисунок 1):
a) наружный диаметр верхней части: 40 мм ± 1,5 мм;
b) внутренний диаметр основания: 20 мм ± 1,5 мм;
c) наружная высота: 40 мм ± 1,5 мм;
d) толщина стенок: менее 2 мм.
2 © ISO 2006 – Все права сохраняются
---------------------- Page: 6 ----------------------
ISO 15585:2006(R)
Размеры в миллиметрах
Рисунок 1 — Тигель и крышка
6.3 Крышка, фарфоровая, толщиной 1,5 мм −2,0 мм с отверстием в центре диаметром 2 мм (см.
Рисунок 1).
6.4 Мешалка, изготовленная из металлической проволоки диаметром 1,0 мм − 1,5 мм, имеющая на
одном конце петлю диаметром 8 мм (см. Рисунок 2).
© ISO 2006 – Все права сохраняются 3
---------------------- Page: 7 ----------------------
ISO 15585:2006(R)
Dimensions in millimetres
Рисунок 2 — Мешалка
1)
6.5 Жаропрочный груз, например, из стали марки Nichrome массой 110 г − 115 г (см. Рисунок 3).
Размеры в миллиметрах
Рисунок 3 —Груз из стали
6.6 Пресс для прессования смеси угля и стандартного антрацита под действием массы 6 кг (см.
Рисунок 4).
1) Марка Nichrome является примером подходящего продукта, имеющегося в продаже. Эта информация
приводится для удобства пользователей ISO 15585 и не означает одобрения этого продукта ISO.
4 © ISO 2006 – Все права сохраняются
---------------------- Page: 8 ----------------------
ISO 15585:2006(R)
Размеры в миллиметрах
Обозначения
1 плита основания 6 приемный стол 11 каретка
2 винт 7 опорный вал 12 рукоятка
3 круглое основание 8 небольшой вал 13 пресс
4 стальная трубка 9 выгрузка 14 ведущий вертикальный вал
5 соединительная планка 10 шплинт 15 пуансон
Рисунок 4 — Пресс, используемый для прессования смеси антрацита и испытательного угля
© ISO 2006 – Все права сохраняются 5
---------------------- Page: 9 ----------------------
ISO 15585:2006(R)
6.7 Электрическая печь с зоной постоянной температуры, оснащенная регулятором температуры,
поддерживающим температуру этой зоны на уровне 850 °C ± 10 °C.
6.8 Барабан с крышкой, приводным валом, передаточным механизмом и электрическим двигателем
для проведения испытания на абразивное истирание на коксе.
Барабан (см. Рисунок 5) имеет внутренний диаметр 200 мм, глубину 70 мм и изготовлен из листового
железа толщиной 3 мм. К внутренним стенкам приварены две симметричные полоски листового
железа длиной 70 мм, шириной 30 мм и толщиной 2 мм. Для закрытия барабана крышка
устанавливается на войлочную или резиновую прокладку и закрепляется двумя крыльчатыми гайками.
Барабан вращается с поворотной цапфой в горизонтальной плоскости со скоростью 50 ± 2 об/мин.
Размеры в миллиметрах
Рисунок 5 — Барабан, используемый в испытаниях
6.9 Лабораторное
...
INTERNATIONAL ISO
STANDARD 15585
First edition
2006-01-15
Hard coal — Determination of caking
index
Houille — Détermination de l'indice d'agglutination
Reference number
ISO 15585:2006(E)
©
ISO 2006
---------------------- Page: 1 ----------------------
ISO 15585:2006(E)
PDF disclaimer
This PDF file may contain embedded typefaces. In accordance with Adobe's licensing policy, this file may be printed or viewed but
shall not be edited unless the typefaces which are embedded are licensed to and installed on the computer performing the editing. In
downloading this file, parties accept therein the responsibility of not infringing Adobe's licensing policy. The ISO Central Secretariat
accepts no liability in this area.
Adobe is a trademark of Adobe Systems Incorporated.
Details of the software products used to create this PDF file can be found in the General Info relative to the file; the PDF-creation
parameters were optimized for printing. Every care has been taken to ensure that the file is suitable for use by ISO member bodies. In
the unlikely event that a problem relating to it is found, please inform the Central Secretariat at the address given below.
© ISO 2006
All rights reserved. Unless otherwise specified, no part of this publication may be reproduced or utilized in any form or by any means,
electronic or mechanical, including photocopying and microfilm, without permission in writing from either ISO at the address below or
ISO's member body in the country of the requester.
ISO copyright office
Case postale 56 • CH-1211 Geneva 20
Tel. + 41 22 749 01 11
Fax + 41 22 749 09 47
E-mail copyright@iso.org
Web www.iso.org
Published in Switzerland
ii © ISO 2006 – All rights reserved
---------------------- Page: 2 ----------------------
ISO 15585:2006(E)
Contents Page
Foreword. iv
1 Scope . 1
2 Normative references . 1
3 Terms and definitions. 1
4 Principle. 1
5 Reagent. 1
6 Apparatus . 2
7 Coal sample. 7
8 Procedure . 7
9 Calculation of result . 7
10 Supplementary test. 8
11 Precision. 8
12 Test report . 8
Annex A (informative) Extraction and preparation of standard anthracite for caking index
determination . 9
Annex B (informative) Quality test for standard anthracite used for caking index determination. 10
© ISO 2006 – All rights reserved iii
---------------------- Page: 3 ----------------------
ISO 15585:2006(E)
Foreword
ISO (the International Organization for Standardization) is a worldwide federation of national standards bodies
(ISO member bodies). The work of preparing International Standards is normally carried out through ISO
technical committees. Each member body interested in a subject for which a technical committee has been
established has the right to be represented on that committee. International organizations, governmental and
non-governmental, in liaison with ISO, also take part in the work. ISO collaborates closely with the
International Electrotechnical Commission (IEC) on all matters of electrotechnical standardization.
International Standards are drafted in accordance with the rules given in the ISO/IEC Directives, Part 2.
The main task of technical committees is to prepare International Standards. Draft International Standards
adopted by the technical committees are circulated to the member bodies for voting. Publication as an
International Standard requires approval by at least 75 % of the member bodies casting a vote.
Attention is drawn to the possibility that some of the elements of this document may be the subject of patent
rights. ISO shall not be held responsible for identifying any or all such patent rights.
ISO 15585 was prepared by Technical Committee ISO/TC 27, Solid mineral fuels, Subcommittee SC 5,
Method of analysis.
iv © ISO 2006 – All rights reserved
---------------------- Page: 4 ----------------------
INTERNATIONAL STANDARD ISO 15585:2006(E)
Hard coal — Determination of caking index
1 Scope
This International Standard specifies a method of determination of caking index of hard coal. It is applicable to
the evaluation of caking power of bituminous coal with random reflectance of vitrinite, R , greater than 0,6 %
r
and less than or equal to 1,8 % (> 0,6 % u 1,8 %).
2 Normative references
The following referenced documents are indispensable for the application of this document. For dated
references, only the edition cited applies. For undated references, the latest edition of the referenced
document (including any amendments) applies.
ISO 562, Hard coal and coke — Determination of volatile matter
ISO 589, Hard coal — Determination of total moisture
ISO 1171, Solid mineral fuels — Determination of ash
3 Terms and definitions
3.1
caking index
measure of the magnitude of the binding strength between coal particles or between coal particles and inert
particles after coal is heated at 850 °C.
4 Principle
A portion of prepared sample of coal of limited size range and the standard anthracite are mixed under
defined conditions, and the mixture is carbonized rapidly. The crucible coke thus obtained is tested for
strength in a drum conforming to certain specifications. The caking power of the test sample is expressed by
the abrasive strength, i.e. resistance to breakage of the crucible coke.
5 Reagent
5.1 Standard anthracite, having a moisture of less than 2,5 mass % air-dried basis, an ash of less than
4 mass % dry basis and a volatile matter of less than 8 mass % dry, ash free basis. The size limits are 0,1 mm
to 0,2 mm, the undersize content of 0,1 mm should not be more than 6 mass % and the oversize content of
0,2 mm should not be more than 4 mass %.
NOTE Annexes A and B provide information on the extraction, preparation and testing of standard anthracite.
© ISO 2006 – All rights reserved 1
---------------------- Page: 5 ----------------------
ISO 15585:2006(E)
6 Apparatus
6.1 Balance, capable of weighing to the nearest 0,01 g.
6.2 Crucible, porcelain, having the following dimensions (see Figure 1):
a) external diameter at the top: 40 mm ± 1,5 mm;
b) internal diameter at the base: 20 mm ± 1,5 mm;
c) external height: 40 mm ± 1,5 mm;
d) wall thickness: less than 2 mm.
2 © ISO 2006 – All rights reserved
---------------------- Page: 6 ----------------------
ISO 15585:2006(E)
Dimensions in millimetres
Figure 1 — Crucible and lid
6.3 Lid, porcelain, 1,5 mm to 2,0 mm thick, with a hole 2 mm in diameter in the centre (see Figure 1).
6.4 Stirrer, made of 1,0 mm to 1,5 mm diameter metal wire, having an 8 mm loop at one end (see Figure 2).
© ISO 2006 – All rights reserved 3
---------------------- Page: 7 ----------------------
ISO 15585:2006(E)
Dimensions in millimetres
Figure 2 — Stirrer
1)
6.5 Heat resistant weight, composed for example of Nichrome steel, with a mass of 110 g to 115 g
(see Figure 3).
Dimensions in millimetres
Figure 3 — Steel weight
6.6 Press, for compressing the mixture of coal and standard anthracite under the weight of a 6 kg mass
(see Figure 4).
1) Nichrome is an example of a suitable product available commercially. This information is given for the convenience of
users of ISO 15585 and does not constitute an endorsement by ISO of this product.
4 © ISO 2006 – All rights reserved
---------------------- Page: 8 ----------------------
ISO 15585:2006(E)
Dimensions in millimetres
Key
1 bottom plate 6 dead plate 11 carriage
2 screw 7 back-up shaft 12 hand knob
3 round base 8 small shaft 13 press
4 steel tube 9 dump 14 lighting vertical shaft
5 connecting board 10 forelock 15 plug
Figure 4 — Press used for compressing the mixture of anthracite and test coal
© ISO 2006 – All rights reserved 5
---------------------- Page: 9 ----------------------
ISO 15585:2006(E)
6.7 Electric furnace, with a zone of uniform temperature and a temperature control device capable of
maintaining that zone at 850 °C ± 10 °C.
6.8 Drum, with a cover, driving shaft, transmission gear and electric motor for carrying out the abrasion test
on coke.
The drum (see Figure 5) has a 200 mm internal diameter, is 70 mm deep and is made of 3 mm thick sheet
iron. To the inside walls are welded two symmetrical sheet iron strips 70 mm long, 30 mm wide and 2 mm
thick. To close the drum, the cover is seated on a felt or rubber gasket and is secured by two wing-nuts.
The drum is rotated with the stub axle horizontal at 50 ± 2 rev/min.
Dimensions in millimetres
Figure
...
SLOVENSKI STANDARD
SIST ISO 15585:2006
01-oktober-2006
ýUQLSUHPRJ±'RORþDQMHNROLþQLNDVSHNDYRVWL
Hard coal -- Determination of caking index
Houille -- Détermination de l'indice d'agglutination
Ta slovenski standard je istoveten z: ISO 15585:2006
ICS:
73.040 Premogi Coals
SIST ISO 15585:2006 en
2003-01.Slovenski inštitut za standardizacijo. Razmnoževanje celote ali delov tega standarda ni dovoljeno.
---------------------- Page: 1 ----------------------
SIST ISO 15585:2006
---------------------- Page: 2 ----------------------
SIST ISO 15585:2006
INTERNATIONAL ISO
STANDARD 15585
First edition
2006-01-15
Hard coal — Determination of caking
index
Houille — Détermination de l'indice d'agglutination
Reference number
ISO 15585:2006(E)
©
ISO 2006
---------------------- Page: 3 ----------------------
SIST ISO 15585:2006
ISO 15585:2006(E)
PDF disclaimer
This PDF file may contain embedded typefaces. In accordance with Adobe's licensing policy, this file may be printed or viewed but
shall not be edited unless the typefaces which are embedded are licensed to and installed on the computer performing the editing. In
downloading this file, parties accept therein the responsibility of not infringing Adobe's licensing policy. The ISO Central Secretariat
accepts no liability in this area.
Adobe is a trademark of Adobe Systems Incorporated.
Details of the software products used to create this PDF file can be found in the General Info relative to the file; the PDF-creation
parameters were optimized for printing. Every care has been taken to ensure that the file is suitable for use by ISO member bodies. In
the unlikely event that a problem relating to it is found, please inform the Central Secretariat at the address given below.
© ISO 2006
All rights reserved. Unless otherwise specified, no part of this publication may be reproduced or utilized in any form or by any means,
electronic or mechanical, including photocopying and microfilm, without permission in writing from either ISO at the address below or
ISO's member body in the country of the requester.
ISO copyright office
Case postale 56 • CH-1211 Geneva 20
Tel. + 41 22 749 01 11
Fax + 41 22 749 09 47
E-mail copyright@iso.org
Web www.iso.org
Published in Switzerland
ii © ISO 2006 – All rights reserved
---------------------- Page: 4 ----------------------
SIST ISO 15585:2006
ISO 15585:2006(E)
Contents Page
Foreword. iv
1 Scope . 1
2 Normative references . 1
3 Terms and definitions. 1
4 Principle. 1
5 Reagent. 1
6 Apparatus . 2
7 Coal sample. 7
8 Procedure . 7
9 Calculation of result . 7
10 Supplementary test. 8
11 Precision. 8
12 Test report . 8
Annex A (informative) Extraction and preparation of standard anthracite for caking index
determination . 9
Annex B (informative) Quality test for standard anthracite used for caking index determination. 10
© ISO 2006 – All rights reserved iii
---------------------- Page: 5 ----------------------
SIST ISO 15585:2006
ISO 15585:2006(E)
Foreword
ISO (the International Organization for Standardization) is a worldwide federation of national standards bodies
(ISO member bodies). The work of preparing International Standards is normally carried out through ISO
technical committees. Each member body interested in a subject for which a technical committee has been
established has the right to be represented on that committee. International organizations, governmental and
non-governmental, in liaison with ISO, also take part in the work. ISO collaborates closely with the
International Electrotechnical Commission (IEC) on all matters of electrotechnical standardization.
International Standards are drafted in accordance with the rules given in the ISO/IEC Directives, Part 2.
The main task of technical committees is to prepare International Standards. Draft International Standards
adopted by the technical committees are circulated to the member bodies for voting. Publication as an
International Standard requires approval by at least 75 % of the member bodies casting a vote.
Attention is drawn to the possibility that some of the elements of this document may be the subject of patent
rights. ISO shall not be held responsible for identifying any or all such patent rights.
ISO 15585 was prepared by Technical Committee ISO/TC 27, Solid mineral fuels, Subcommittee SC 5,
Method of analysis.
iv © ISO 2006 – All rights reserved
---------------------- Page: 6 ----------------------
SIST ISO 15585:2006
INTERNATIONAL STANDARD ISO 15585:2006(E)
Hard coal — Determination of caking index
1 Scope
This International Standard specifies a method of determination of caking index of hard coal. It is applicable to
the evaluation of caking power of bituminous coal with random reflectance of vitrinite, R , greater than 0,6 %
r
and less than or equal to 1,8 % (> 0,6 % u 1,8 %).
2 Normative references
The following referenced documents are indispensable for the application of this document. For dated
references, only the edition cited applies. For undated references, the latest edition of the referenced
document (including any amendments) applies.
ISO 562, Hard coal and coke — Determination of volatile matter
ISO 589, Hard coal — Determination of total moisture
ISO 1171, Solid mineral fuels — Determination of ash
3 Terms and definitions
3.1
caking index
measure of the magnitude of the binding strength between coal particles or between coal particles and inert
particles after coal is heated at 850 °C.
4 Principle
A portion of prepared sample of coal of limited size range and the standard anthracite are mixed under
defined conditions, and the mixture is carbonized rapidly. The crucible coke thus obtained is tested for
strength in a drum conforming to certain specifications. The caking power of the test sample is expressed by
the abrasive strength, i.e. resistance to breakage of the crucible coke.
5 Reagent
5.1 Standard anthracite, having a moisture of less than 2,5 mass % air-dried basis, an ash of less than
4 mass % dry basis and a volatile matter of less than 8 mass % dry, ash free basis. The size limits are 0,1 mm
to 0,2 mm, the undersize content of 0,1 mm should not be more than 6 mass % and the oversize content of
0,2 mm should not be more than 4 mass %.
NOTE Annexes A and B provide information on the extraction, preparation and testing of standard anthracite.
© ISO 2006 – All rights reserved 1
---------------------- Page: 7 ----------------------
SIST ISO 15585:2006
ISO 15585:2006(E)
6 Apparatus
6.1 Balance, capable of weighing to the nearest 0,01 g.
6.2 Crucible, porcelain, having the following dimensions (see Figure 1):
a) external diameter at the top: 40 mm ± 1,5 mm;
b) internal diameter at the base: 20 mm ± 1,5 mm;
c) external height: 40 mm ± 1,5 mm;
d) wall thickness: less than 2 mm.
2 © ISO 2006 – All rights reserved
---------------------- Page: 8 ----------------------
SIST ISO 15585:2006
ISO 15585:2006(E)
Dimensions in millimetres
Figure 1 — Crucible and lid
6.3 Lid, porcelain, 1,5 mm to 2,0 mm thick, with a hole 2 mm in diameter in the centre (see Figure 1).
6.4 Stirrer, made of 1,0 mm to 1,5 mm diameter metal wire, having an 8 mm loop at one end (see Figure 2).
© ISO 2006 – All rights reserved 3
---------------------- Page: 9 ----------------------
SIST ISO 15585:2006
ISO 15585:2006(E)
Dimensions in millimetres
Figure 2 — Stirrer
1)
6.5 Heat resistant weight, composed for example of Nichrome steel, with a mass of 110 g to 115 g
(see Figure 3).
Dimensions in millimetres
Figure 3 — Steel weight
6.6 Press, for compressing the mixture of coal and standard anthracite under the weight of a 6 kg mass
(see Figure 4).
1) Nichrome is an example of a suitable product available commercially. This information is given for the convenience of
users of ISO 15585 and does not constitute an endorsement by ISO of this product.
4 © ISO 2006 – All rights reserved
---------------------- Page: 10 ----------------------
SIST ISO 15585:2006
ISO 15585:2006(E)
Dimensions in millimetres
Key
1 bottom plate 6 dead plate 11 carriage
2 screw 7 back-up shaft 12 hand knob
3 round base 8 small shaft 13 press
4 steel tube 9 dump 14 lighting vertical shaft
5 connecting board 10 forelock 15 plug
Figure 4 — Press used for compressing the mixture of anthracite and test coal
© ISO 2006 – All rights reserved 5
---------------------- Page: 11 ----------------------
SIST ISO 15585:2006
ISO 15585:2006(E)
6.7 Electric furnace, with a zone of uniform temperature and a temperature control device capable of
maintaining that zone at 850 °C ± 10 °C.
6.8 Drum, with a cover, driving shaft, transmission gear and electric motor for carrying out the abrasion test
on coke.
The drum (see F
...
Questions, Comments and Discussion
Ask us and Technical Secretary will try to provide an answer. You can facilitate discussion about the standard in here.