Corrosion of metals and alloys — Stress corrosion testing — Part 6: Preparation and use of precracked specimens for tests under constant load or constant displacement

This document specifies procedures for designing, preparing and using precracked specimens for investigating susceptibility to stress corrosion. It gives recommendations for the design, preparation and use of precracked specimens for investigating susceptibility to stress corrosion. Recommendations concerning notched specimens are given in Annex A. The term "metal" as used in this document includes alloys. Because of the need to confine plasticity at the crack tip, precracked specimens are not suitable for the evaluation of thin products, such as sheet or wire, and are generally used for thicker products including plate bar and forgings. They can also be used for parts joined by welding. Precracked specimens can be loaded with equipment for application of a constant load or can incorporate a device to produce a constant displacement at the loading points. Tests conducted under increasing displacement or increasing load are dealt with in ISO 7539-9. A particular advantage of precracked specimens is that they allow data to be acquired, from which critical defect sizes, above which stress corrosion cracking can occur, can be estimated for components of known geometry subjected to known stresses. They also enable rates of stress corrosion crack propagation to be determined. The latter data can be taken into account when monitoring parts containing defects during service.

Corrosion des métaux et alliages — Essais de corrosion sous contrainte — Partie 6: Préparation et utilisation des éprouvettes préfissurées pour essais sous charge constante ou sous déplacement constant

Le présent document spécifie les procédures de conception, de préparation et d'utilisation d'éprouvettes préfissurées servant à évaluer la sensibilité à la corrosion sous contrainte. Il donne des recommandations pour la conception, la préparation et l'utilisation d'éprouvettes préfissurées pour évaluer la sensibilité à la corrosion sous contrainte. Des recommandations relatives aux éprouvettes entaillées sont données dans l'Annexe A. Pour les besoins du présent document, le terme « métal » inclut également les alliages. Comme il est nécessaire de confiner la déformation plastique en fond de fissure, les éprouvettes préfissurées ne se prêtent pas à l'évaluation des produits minces tels que les tôles minces et les fils, et sont généralement utilisées pour des produits plus épais tels que les tôles en barres et les pièces forgées. Elles peuvent aussi être utilisées pour des pièces assemblées par soudage. Les éprouvettes préfissurées peuvent être soumises à une contrainte à l'aide d'appareils exerçant une charge constante ou comprenant un dispositif qui engendre un déplacement constant des points d'application de la charge. Les essais sous déplacement croissant ou sous charge croissante sont traités dans l'ISO 7539‑9. Les éprouvettes préfissurées présentent l'avantage de permettre l'acquisition de données dont on peut déduire les tailles critiques de défaut au-delà desquelles une fissuration par corrosion sous contrainte peut se produire au niveau de pièces de géométrie connue soumises à des efforts connus. Ces éprouvettes permettent également de déterminer la vitesse de propagation des fissures de corrosion sous contrainte. Ces dernières données peuvent être prises en compte dans le cadre de la surveillance en service de pièces comportant des défauts.

General Information

Status
Published
Publication Date
21-Aug-2018
Current Stage
9060 - Close of review
Start Date
04-Mar-2029
Ref Project

Relations

Buy Standard

Standard
ISO 7539-6:2018 - Corrosion of metals and alloys -- Stress corrosion testing
English language
40 pages
sale 15% off
Preview
sale 15% off
Preview
Standard
ISO 7539-6:2018 - Corrosion des métaux et alliages -- Essais de corrosion sous contrainte
French language
43 pages
sale 15% off
Preview
sale 15% off
Preview

Standards Content (Sample)

INTERNATIONAL ISO
STANDARD 7539-6
Fourth edition
2018-08
Corrected version
2018-11
Corrosion of metals and alloys —
Stress corrosion testing —
Part 6:
Preparation and use of precracked
specimens for tests under constant
load or constant displacement
Corrosion des métaux et alliages — Essais de corrosion sous
contrainte —
Partie 6: Préparation et utilisation des éprouvettes préfissurées pour
essais sous charge constante ou sous déplacement constant
Reference number
ISO 7539-6:2018(E)
©
ISO 2018

---------------------- Page: 1 ----------------------
ISO 7539-6:2018(E)

COPYRIGHT PROTECTED DOCUMENT
© ISO 2018
All rights reserved. Unless otherwise specified, or required in the context of its implementation, no part of this publication may
be reproduced or utilized otherwise in any form or by any means, electronic or mechanical, including photocopying, or posting
on the internet or an intranet, without prior written permission. Permission can be requested from either ISO at the address
below or ISO’s member body in the country of the requester.
ISO copyright office
CP 401 • Ch. de Blandonnet 8
CH-1214 Vernier, Geneva
Phone: +41 22 749 01 11
Fax: +41 22 749 09 47
Email: copyright@iso.org
Website: www.iso.org
Published in Switzerland
ii © ISO 2018 – All rights reserved

---------------------- Page: 2 ----------------------
ISO 7539-6:2018(E)

Contents Page
Foreword .iv
1 Scope . 1
2 Normative references . 1
3 Terms and definitions . 1
4 Principle . 4
5 Specimens . 5
5.1 General . 5
5.2 Specimen design . 7
5.3 Stress intensity factor considerations . .17
5.4 Specimen preparation .23
5.5 Specimen identification .25
6 Initiation and propagation of fatigue cracks .25
7 Procedure.27
7.1 General .27
7.2 Environmental considerations .27
7.3 Environmental chamber .28
7.4 Environmental control and monitoring .29
7.5 Determination of K by crack arrest .
...

NORME ISO
INTERNATIONALE 7539-6
Quatrième édition
2018-08
Version corrigée
2018-11
Corrosion des métaux et alliages —
Essais de corrosion sous contrainte —
Partie 6:
Préparation et utilisation des
éprouvettes préfissurées pour
essais sous charge constante ou sous
déplacement constant
Corrosion of metals and alloys — Stress corrosion testing —
Part 6: Preparation and use of precracked specimens for tests under
constant load or constant displacement
Numéro de référence
ISO 7539-6:2018(F)
©
ISO 2018

---------------------- Page: 1 ----------------------
ISO 7539-6:2018(F)

DOCUMENT PROTÉGÉ PAR COPYRIGHT
© ISO 2018
Tous droits réservés. Sauf prescription différente ou nécessité dans le contexte de sa mise en œuvre, aucune partie de cette
publication ne peut être reproduite ni utilisée sous quelque forme que ce soit et par aucun procédé, électronique ou mécanique,
y compris la photocopie, ou la diffusion sur l’internet ou sur un intranet, sans autorisation écrite préalable. Une autorisation peut
être demandée à l’ISO à l’adresse ci-après ou au comité membre de l’ISO dans le pays du demandeur.
ISO copyright office
Case postale 401 • Ch. de Blandonnet 8
CH-1214 Vernier, Genève
Tél.: +41 22 749 01 11
Fax: +41 22 749 09 47
E-mail: copyright@iso.org
Web: www.iso.org
Publié en Suisse
ii © ISO 2018 – Tous droits réservés

---------------------- Page: 2 ----------------------
ISO 7539-6:2018(F)

Sommaire Page
Avant-propos .iv
1 Domaine d'application . 1
2 Références normatives . 1
3 Termes et définitions . 1
4 Principe . 4
5 Éprouvettes . 5
5.1 Généralités . 5
5.2 Modèle d’éprouvette . 7
5.3 Considérations concernant le facteur d’intensité de contrainte .18
5.4 Préparation des éprouvettes .24
5.5 Identification des éprouvettes .26
6 Amorçage et propagation de la fissure de fatigue .26
7 Mode opératoire.28
7.1 Généralités .28
7.2 Considérations environnementales .28
7.3 Enceinte environnementale .29
7.4 Contrôle et surveillance du milieu .30
7.5 Détermination de K par la méthode d’arrêt de la fissuration.31
ISCC
7.6 Détermination de K par amorçage de la fissure .
...

Questions, Comments and Discussion

Ask us and Technical Secretary will try to provide an answer. You can facilitate discussion about the standard in here.