Paper and board - Determination of tensile properties - Part 2: Constant rate of elongation method (20 mm/min) (ISO 1924-2:2008)

ISO 1924-2:2008 specifies a method for measuring the tensile strength, strain at break and tensile energy absorption of paper and board, using a testing machine operating at a constant rate of elongation (20 mm/min). ISO 1924-2:2008 also specifies equations for calculating the tensile index, the tensile energy absorption index and the modulus of elasticity.
Testing in conformance with ISO 1924-2:2008 always includes the measurement of tensile strength. Measurement or calculation of other properties is subject to agreement between the parties concerned.
ISO 1924-2:2008 is applicable to all papers and boards, including papers with a high strain at break if the results are within the capacity of the testing machine. It also applies to the components of corrugated board but not, however, to corrugated board itself.

Papier und Pappe - Bestimmung von Eigenschaften bei Zugbeanspruchung - Teil 2: Verfahren mit konstanter Dehngeschwindigkeit (20 mm/min) (ISO 1924-2:2008)

Dieser Teil der ISO 1924 legt ein Verfahren fest, mit dem die breitenbezogene Bruchkraft und die Bruchdehnung sowie das Arbeitsaufnahmevermögen bei Zugbeanspruchung von Papier und Pappe gemessen werden. Dabei wird ein Prüfgerät verwendet, das mit konstanter Dehngeschwindigkeit arbeitet (20 mm/min). Weiterhin werden Gleichungen beschrieben, mit denen der Bruchkraftindex, der Arbeitsaufnahmevermögen-Index und der Elastizitätsmodul berechnet werden können.
Prüfungen mit Bezug auf diesen Teil der ISO 1924 schließen immer die Bestimmung der breitenbezogenen Bruchkraft mit ein. Die Messung und Berechnung anderer Eigenschaften muss stets zwischen den betroffenen Parteien vereinbart werden.
Dieser Teil von ISO 1924 ist anwendbar auf alle Papiere und Pappen, eingeschlossen Papiere mit hoher Bruchdehnung, falls der Bereich durch das Prüfgerät abgedeckt ist. Er ist auch auf einzelne Komponenten von Wellpappe anwendbar, jedoch nicht auf die Wellpappe selbst.
Dieser Teil der ISO 1924 ist nicht auf Tissue-Papier und Tissue-Produkte anwendbar. Hierfür gilt ISO 12625 4 [2].
Für die Bestimmung von Eigenschaften bei Zugbeanspruchung an Laborblättern wird ISO 5270 [3] empfohlen.

Papier et carton - Détermination des propriétés de traction - Partie 2: Méthode à gradient d'allongement constant (20 mm/min) (ISO 1924-2:2008)

L'ISO 1924-2:2008 spécifie une méthode de mesurage de la résistance à la rupture par traction, de la déformation à la rupture et de l'énergie absorbée à la rupture par traction des papiers et cartons, à l'aide d'un appareil d'essai à gradient d'allongement constant (20 mm/min). L'ISO 1924-2:2008 spécifie également des équations pour le calcul de l'indice de rupture par traction, de l'indice d'énergie absorbée à la rupture par traction et du module d'élasticité.
Les essais réalisés conformément à l'ISO 1924-2:2008 comprennent toujours le mesurage de la résistance à la rupture par traction. Le mesurage ou le calcul d'autres propriétés est soumis à accord entre les parties intéressées.
L'ISO 1924-2:2008 est applicable à tous les papiers et cartons, y compris aux papiers à forte déformation à la rupture, si les résultats s'inscrivent dans les limites de la capacité de l'appareil d'essai. Elle s'applique également aux composants du carton ondulé mais cependant, pas au carton ondulé lui-même.

Papir, karton in lepenka - Določevanje nateznih lastnosti - 2. del: Metoda z enakomernim naraščanjem raztezka (20 mm/min) (ISO 1924-2:2008)

General Information

Status
Published
Publication Date
14-Dec-2008
Current Stage
9093 - Decision to confirm - Review Enquiry
Start Date
02-May-2014
Completion Date
02-May-2014

Relations

Buy Standard

Standard
EN ISO 1924-2:2009
English language
20 pages
sale 10% off
Preview
sale 10% off
Preview
e-Library read for
1 day

Standards Content (Sample)


2003-01.Slovenski inštitut za standardizacijo. Razmnoževanje celote ali delov tega standarda ni dovoljeno.Papier und Pappe - Bestimmung von Eigenschaften bei Zugbeanspruchung - Teil 2: Verfahren mit konstanter Dehngeschwindigkeit (20 mm/min) (ISO 1924-2:2008)Papier et carton - Détermination des propriétés de traction - Partie 2: Méthode à gradient d'allongement constant (20 mm/min) (ISO 1924-2:2008)Paper and board - Determination of tensile properties - Part 2: Constant rate of elongation method (20 mm/min) (ISO 1924-2:2008)85.060Papir, karton in lepenkaPaper and boardICS:Ta slovenski standard je istoveten z:EN ISO 1924-2:2008SIST EN ISO 1924-2:2009en,fr,de01-april-2009SIST EN ISO 1924-2:2009SLOVENSKI
STANDARDSIST EN ISO 1924-2:20001DGRPHãþD

EUROPEAN STANDARDNORME EUROPÉENNEEUROPÄISCHE NORMEN ISO 1924-2December 2008ICS 85.060Supersedes EN ISO 1924-2:1995
English VersionPaper and board - Determination of tensile properties - Part 2:Constant rate of elongation method (20 mm/min) (ISO 1924-2:2008)Papier et carton - Détermination des propriétés de traction -Partie 2: Méthode à gradient d'allongement constant (20mm/min) (ISO 1924-2:2008)Papier und Pappe - Bestimmung von Eigenschaften beiZugbeanspruchung - Teil 2: Verfahren mit konstanterDehngeschwindigkeit (20 mm/min)
(ISO 1924-2:2008)This European Standard was approved by CEN on 19 November 2008.CEN members are bound to comply with the CEN/CENELEC Internal Regulations which stipulate the conditions for giving this EuropeanStandard the status of a national standard without any alteration. Up-to-date lists and bibliographical references concerning such nationalstandards may be obtained on application to the CEN Management Centre or to any CEN member.This European Standard exists in three official versions (English, French, German). A version in any other language made by translationunder the responsibility of a CEN member into its own language and notified to the CEN Management Centre has the same status as theofficial versions.CEN members are the national standards bodies of Austria, Belgium, Bulgaria, Cyprus, Czech Republic, Denmark, Estonia, Finland,France, Germany, Greece, Hungary, Iceland, Ireland, Italy, Latvia, Lithuania, Luxembourg, Malta, Netherlands, Norway, Poland, Portugal,Romania, Slovakia, Slovenia, Spain, Sweden, Switzerland and United Kingdom.EUROPEAN COMMITTEE FOR STANDARDIZATIONCOMITÉ EUROPÉEN DE NORMALISATIONEUROPÄISCHES KOMITEE FÜR NORMUNGManagement Centre:
Avenue Marnix 17,
B-1000 Brussels© 2008 CENAll rights of exploitation in any form and by any means reservedworldwide for CEN national Members.Ref. No. EN ISO 1924-2:2008: ESIST EN ISO 1924-2:2009

Reference numberISO 1924-2:2008(E)© ISO 2008
INTERNATIONAL STANDARD ISO1924-2Third edition2008-12-15Paper and board — Determination of tensile properties — Part 2: Constant rate of elongation method (20 mm/min) Papier et carton — Détermination des propriétés de traction — Partie 2: Méthode à gradient d'allongement constant (20 mm/min)
ISO 1924-2:2008(E) PDF disclaimer This PDF file may contain embedded typefaces. In accordance with Adobe's licensing policy, this file may be printed or viewed but shall not be edited unless the typefaces which are embedded are licensed to and installed on the computer performing the editing. In downloading this file, parties accept therein the responsibility of not infringing Adobe's licensing policy. The ISO Central Secretariat accepts no liability in this area. Adobe is a trademark of Adobe Systems Incorporated. Details of the software products used to create this PDF file can be found in the General Info relative to the file; the PDF-creation parameters were optimized for printing. Every care has been taken to ensure that the file is suitable for use by ISO member bodies. In the unlikely event that a problem relating to it is found, please inform the Central Secretariat at the address given below.
©
ISO 2008 All rights reserved. Unless otherwise specified, no part of this publication may be reproduced or utilized in any form or by any means, electronic or mechanical, including photocopying and microfilm, without permission in writing from either ISO at the address below or ISO's member body in the country of the requester. ISO copyright office Case postale 56 • CH-1211 Geneva 20 Tel.
+ 41 22 749 01 11 Fax
+ 41 22 749 09 47 E-mail
copyright@iso.org Web
www.iso.org Published in Switzerland
ii © ISO 2008 – All rights reserved
ISO 1924-2:2008(E) © ISO 2008 – All rights reserved iii Contents Page Foreword.iv Introduction.v 1 Scope.1 2 Normative references.1 3 Terms and definitions.2 4 Principle.2 5 Apparatus.3 6 Calibration and adjustment of apparatus.4 7 Sampling and preparation of test pieces.4 7.1 Sampling.4 7.2 Conditioning.4 7.3 Preparation of test pieces.5 8 Procedure.5 9 Calculation and report.6 9.1 General.6 9.2 Tensile strength.6 9.3 Tensile index.6 9.4 Strain at break.6 9.5 Tensile energy absorption.7 9.6 Tensile energy absorption index.7 9.7 Modulus of elasticity.7 10 Precision.8 10.1 General.8 10.2 Repeatability.8 10.3 Reproducibility.8 11 Test report.10 Annex A (normative)
Calibration of the tensile testing machine.11 Bibliography.12
ISO 1924-2:2008(E) iv © ISO 2008 – All rights reserved Foreword ISO (the International Organization for Standardization) is a worldwide federation of national standards bodies (ISO member bodies). The work of preparing International Standards is normally carried out through ISO technical committees. Each member body interested in a subject for which a technical committee has been established has the right to be represented on that committee. International organizations, governmental and non-governmental, in liaison with ISO, also take part in the work. ISO collaborates closely with the International Electrotechnical Commission (IEC) on all matters of electrotechnical standardization. International Standards are drafted in accordance with the rules given in the ISO/IEC Directives, Part 2. The main task of technical committees is to prepare International Standards. Draft International Standards adopted by the technical committees are circulated to the member bodies for voting. Publication as an International Standard requires approval by at least 75 % of the member bodies casting a vote. Attention is drawn to the possibility that some of the elements of this document may be the subject of patent rights. ISO shall not be held responsible for identifying any or all such patent rights. ISO 1924-2 was prepared by Technical Committee ISO/TC 6, Paper, board and pulps, Subcommittee SC 2, Test methods and quality specifications for paper and board. This third edition cancels and replaces the second edition (ISO 1924-2:1994), which has been technically revised with respect to terms and definitions (in order to be in line with the terms and definitions used in ISO 1924-3[1]). The numbering of clauses and their contents have been changed to be congruent with ISO 1924-3. ISO 1924 consists of the following parts, under the general title Paper and board — Determination of tensile properties1): ⎯ Part 2: Constant rate of elongation method (20 mm/min) ⎯ Part 3: Constant rate of elongation method (100 mm/min)
1) ISO 1924-1, Constant rate of loading method, was withdrawn in 2004 as it was considered obsolete. SIST EN ISO 1924-2:2009

ISO 1924-2:2008(E) © ISO 2008 – All rights reserved v Introduction The method for determination of tensile properties specified in this part of ISO 1924 is the one most commonly used. It is related to the method specified in ISO 1924-3. In this part of ISO 1924 (ISO 1924-2), the constant rate of elongation applied is 20 mm/min, whereas in ISO 1924-3, the constant rate of elongation applied is 100 mm/min. Since the results of a tensile test depend on the rate of elongation applied, this part of ISO 1924 and ISO 1924-3 will not give the same results. The rate dependence can vary according to paper grade and is different for tensile strength, strain at break, tensile energy absorption and modulus of elasticity. NOTE 1 In most cases, the tensile properties can increase by 5 % to 15 % when the rate of elongation is increased from 20 mm/min (180 mm test span length) to 100 mm/min (100 mm test span length). NOTE 2 In this part of ISO 1924, the same terminology and symbols are used as in ISO 1924-3 and in general literature concerning materials physics and mechanics.
INTERNATIONAL STANDARD ISO 1924-2:2008(E) © ISO 2008 – All rights reserved 1 Paper and board — Determination of tensile properties — Part 2: Constant rate of elongation method (20 mm/min) 1 Scope This part of ISO 1924 specifies a method for measuring the tensile strength, strain at break and tensile energy absorption of paper and board, using a testing machine operating at a constant rate of elongation (20 mm/min). This part of ISO 1924 also specifies equations for calculating the tensile index, the tensile energy absorption index and the modulus of elasticity. Testing in conformance with this part of ISO 1924 always includes the measurement of tensile strength. Measurement or calculation of other properties is subject to agreement between the parties concerned. This part of ISO 1924 is applicable to all papers and boards, including papers with a high strain at break if the results are within the capacity of the testing machine. It also applies to the components of corrugated board but not, however, to corrugated board itself. This part of ISO 1924 is not applicable to tissue paper and tissue products
...

Questions, Comments and Discussion

Ask us and Technical Secretary will try to provide an answer. You can facilitate discussion about the standard in here.